 low smoke halogen-free flame retardant polyolefin compound jacket material for power cable  low smoke halogen-free flame retardant polyolefin compound jacket material for power cable  low smoke halogen-free flame retardant polyolefin compound jacket material for power cable
Next

low smoke halogen-free flame retardant polyolefin compound jacket material for power cable

离岸价格

Get Latest Price

1.1 ~ 1.6 USD / Kilogram

|

1000 Kilogram Minimum Order

国:

China

モデル番号:

SHD 01-H-02

离岸价格:

1.1 ~ 1.6 USD / Kilogram Get Latest Price

ロケーション:

Yuanshi country, Hebei Province, China

最低注文量の価格:

1.1 per Kilogram

最低注文量:

1000 Kilogram

パッケージの詳細:

Packing: N. W: 25kg/1000kg bags with inner bag of aluminum -plastic composite vacuum

納期:

7-15 days

供給能力:

10000000 Kilogram per Week

支払いタイプ:

T/T

今すぐお問い合わせください
無料会員

連絡先担当者 Tina

Shijiazhuang, Hebei

今すぐお問い合わせください

製品仕様

  • Density:1.45g/cm3
  • Hardness (Shore D):58
  • Tensile strength:12.5Mpa
  • Elongation at break:215%
  • Tensile strength after aging:11.3Mpa
  • Rate of change in tensile strength:+15
  • Oxygen Index :38.5
  • Halogen acid gas release amount:0 mg/g
  • Tpxicity index:0.5

タイトルまたは説明

Sell cable compound material
Thermoplastic low smoke halogen-free flame retardant polyolefin compound jacket material for power cable

Standard: GB/T*********5, IEC*************9
1. The product not only has excellent low-smoke halogen-free flame retardant performance,but also has excellent extrusiion processing performance. It can be extruded on an ordinary PVC extruder. As long as the cooling device is normal, the extrusion processing speed can be accelerated. The performance of thid product is batter than similar products.

  The series are based on polyolefin and contain special halogen-free flame retardants and smoke suppresants,which are processed by precise mixing with special formulas. When the cable structure is desugned reasonably, it can pass the A/B/C type combustion test and meet the light transmittance requirments. When burning, no halogen acid gas is released, the amound of toxic and crossive gas is vey small and the smokeconcentration is very low. We can also provide anti-termite, anti-rodent and UV resistant properties according to customer requirment.

2.Feature ans uses
This product is suitable for accasions with high flame retardant requirments and low secondary hazards, such as subways, ships, high-rise building program-controlled switch rooms, computer rooms and various crowded public places. Suitabke for optical cable and wire core working termperature *0℃ low smoke halogen free flame retardant cable sheath. This product is guaranteed to pass verious beam burning tests and light transmittance tests. What's more, it has super cracking resistance property.

3. Extrusion process
The drying temperature is *5℃ and the drying time is at least 2 hours. It is advisable for the hot material to enter the extruder. It can be extruded by L/D ****5 extruder. When the screw compression ratio is low, the output volume is large. Ecah zone of the extruder must have a cooling control system and the indicated value of the temperaturecontrol table varis with the typr of extruder, each user should select a suitable temperature according to the specific conditions of the extruder used. The following temperatures can be used as a referancefor commissioning:
The following temperatures can be used as a reference for commissioning:

Barrel position Zone 1 Zone 2 Zone 3 Zone 4 nose and mode
temperature(℃) **5±5 **5±5 **5±5 **5±5        **0±5
The machine head can be withour a filter screen or a filter screen below *0 mesh can be used. It can be matched with special color masterbatch, the dosage is about **2%, generally does not affect the materials properties
Note: If the aluminum-plastic composite inner bag's damp proof fails, it should be dried before use. The drying temperature should be *5℃ ad the drying time should be at least 2 hours. It is better for hot material to enter and leave the extruder.
4. Packaging, transportation and storage:
Packing: N. W: *5kg/***0kg bags with inner bag of aluminum -plastic composite vacuum moisture-proof bag and outer packing being made of kraft paper composite bag or woven bag. It should not be exposed to the sun and the rain during transport. It should be stored in a clean, cool, dry and ventilated warehouse. It should be handled with care.
5. Shelf life: 6 months

国: China
モデル番号: SHD 01-H-02
离岸价格: 1.1 ~ 1.6 / Kilogram Get Latest Price
ロケーション: Yuanshi country, Hebei Province, China
最低注文量の価格: 1.1 per Kilogram
最低注文量: 1000 Kilogram
パッケージの詳細: Packing: N. W: 25kg/1000kg bags with inner bag of aluminum -plastic composite vacuum
納期: 7-15 days
供給能力: 10000000 Kilogram per Week
支払いタイプ: T/T
製品グループ : thermoplastic LSZH cable material

Send a direct inquiry to this supplier

To:

Tina < Hebei Sunua Advanced Material Co., ltd >

私は知りたい: