Ordinary Glass Frosting Powder
Next

Ordinary Glass Frosting Powder

离岸价格

Get Latest Price

|

- Minimum Order

国:

China

モデル番号:

ST-101

离岸价格:

Get Latest Price

ロケーション:

-

最低注文量の価格:

-

最低注文量:

-

パッケージの詳細:

-

納期:

-

供給能力:

-

支払いタイプ:

-

製品グループ :

-

今すぐお問い合わせください

連絡先担当者 bai

Songtao road, Shanghai, Shanghai

今すぐお問い合わせください

製品仕様

タイトルまたは説明

Common Glass Frosting Powder ST***1 can frost Sodium-Calcium-Silicon glass such as lamp glass, flat glass, bottles, arts ***** ST***1 is based on industrial grade Hydrochloric Acid. It is a new type environment-friendly powder that allows a better recycling . Stable and easy to use the powder makes your glass appears softer and white.


Frosting Operation >> Preparation of the Frosting Solution
·Mature the Frosting solution at least *4 hours before use
.
·The ratio of powder ST***1 to Hydrochloric Acid
 (≥*1) is 1:0.*0.
·Keep the powder in a plastic container, slowly pour Hydrochloric
  Acid in, and keep stirring the solution evenly. Finally, cover
  the container.
·Keep maturation over *4 hours before use (The longer, the better)
·The newly-prepared solution is too thick, and its temperature
 will fall down slowly, so don"t apply it until it comes back to
 be normal in temperature and thickness.

Frosting Operation >>Frosting Process
·Constantly stir the matured solution to be even completely
.
·Dip the clean glass wares into the solution for ****0 seconds
.
· Take out the etched glass to drop for ****0 seconds
.
·In the beginning, the solution is fairly thick. However the
 etching time should be longer when the solution becomes less
 thick after etching for some time. 
·The frosting time varies with the temperature and chemical
 compositions.
·For dirty glass, use *5 Hydrochloric Acid to wash.

Frosting Operation >>Wash Process & Dry
 · Rinse and wash the frosted glass wares under the running water
· Dip the glass into the ***0 diluted Hydrochloric Acid for ****0
 seconds to make brasive parparticles on the glass easy to
 remove.
·Rinse and wash the glass again under the running water
 and dry it with air for package.

国: China
モデル番号: ST-101
离岸价格: Get Latest Price
ロケーション: -
最低注文量の価格: -
最低注文量: -
パッケージの詳細: -
納期: -
供給能力: -
支払いタイプ: -
製品グループ : -
Ordinary Glass Frosting Powder

Send a direct inquiry to this supplier

To:

bai < torlin chemicals >

私は知りたい: